Specifications include, but are not limited to: The recommended specification limits for the asphalt crack seal material when heated in accordance with ASTM D5078 to the maximum heating temperature are as follows: Test ASTM Recommended Specification Cone Penetration D5329 20-40 Resilience D5329 30% min. Softening Point D36 210F (99C) min. Ductility 77F (25C) D113 30 cm min. Flexibility 1/8" (3.2mm) specimen, 90-degree bend, 10 sec., 1" (25mm) mandrel D3111 Modified Flow 140F (60C), 5h D5329 Pass at 30F (- 1C) Viscosity 400F (204C) D2669 3 mm max Asphalt Compatibility D5329 100 Poise max. Bitumen Content D4 Pass Tensile Adhesion 1" (25.4 mm) thickness D5329 60% Min. Maximum Heating Temperature 400F (204C) Minimum Application Temperature 380F (193C).