Specifications include, but are not limited to: The crushed recycled asphalt shall consist of crushed gravel, rock, sand, or other approved material furnished by the Municipality. The aggregate shall be derived from recovered AC pavement and various other materials on site and be free from lumps, balls of clay, deleterious, or other objectionable matter and shall be durable and sound. Maximum RAP conglomerate (prior to extraction) shall pass the 1" sieve. ; Asphalt content (by weight of total mix) shall be 2.7 percent to 4.7 percent. The asphalt content of RAP delivered shall be determined on individual extraction test results and not an average of extractions conducted. The RAP shall be measured in tons of materials delivered. Said measurement may include moisture up to a maximum of 3.5 percent of dry weight of the material. ;